Rozsah specifikací pro potrubí A333 LTCS
Dec 02, 2024
|
Stupeň |
Rozsah specifikace |
Norma |
||
|
OD /mm |
WT /mm |
Délka/m |
||
|
A333 Gr.6
A333 Gr.6/X42NS
|
10-127 |
1-20 |
6-12.0 |
ASTM A333
Standardní specifikace pro bezešvé a svařované ocelové trubky pro kryogenní operace |
|
42-114.3 |
3.5-6 |
6-12.2 |
||
|
42-114.3 |
6-12 |
6-12.2 |
||
|
114.3-180 |
3.8-8 |
6-12.2 |
||
|
114.3-180 |
8-22 |
6-12.2 |
||
|
68-180 |
10-14 |
6-12.2 |
||
|
69-254 |
14-55 |
6-12.2 |
||
|
140-340 |
6-8 |
6-12.2 |
||
|
140-368 |
8-42 |
6-12.2 |
||
|
318-720 |
14-50 |
4-12.5 |
||
|
A333 Gr.6/X52QS |
42-114.3 |
3.5-12 |
6-12.2 |
|
|
114.3-180 |
3.8-22 |
6-12.2 |
||
|
68-254 |
10-40 |
6-12.2 |
||
|
140-368 |
6-40 |
6-12.2 |
||
|
318-720 |
14-40 |
4-12.5 |
||
|
140-368 |
6-25 |
6-12.2 |
||
|
318-720 |
14-25 |
4-12.5 |
||
Prodám hliníkovou trubku GNEE A333